1) Short Introduction:
Surface Finish:3.2um Ra Or As Required.Forging Reduction Min:3 Or As RequiredRought machining or Finis Machining
2) 21CrMoNiV4-7/1.6981 Chemical Composition:
C
Si
Mn
P
S
Cr
Mo
Ni
V
Al
0.17~0.25
0.15~0.35
0.25~0.85
≤0.020
≤0.020
0.9~1.2
0.65~0.80
0.50~0.80
0.25~0.35
≤0.015
1)The Al content of the cast shall be reported and indicated in the certificate3) Heat Treatment:
Hardening:
900-950℃/air,oil or water dipping
Tempering:
:680-720℃(2h min)
4) Certfiticates List:
Certificates list
ISO9001:2008
ISO14001:2004
PED Certificate
ABS Certficate
BV Certficate
DNV Certificate
RINA Certficate
GL Certficate
LR Certficate
CCS Certficate
NK Certficate
KR Certficate
API-6A Certficate
API-17D Certficate
CNAS Certficate
5) The main manufacturing equipments:
Name&Description
Capacity
Quantity
3600Thydraulic press
Max. single forging in 18T
1
2000T hydraulic press
Max. single forging in 9T
2
800 h…